Application of Welding Technology for a Zirconium Alloy of Nuclear Fuel Cladding
Soo-Sung Kim, Jin-Hyun Koh, Jung-Won Lee, Geun-Il Park
J Weld Join. 2011;29(1):5-8.   Published online March 4, 2011
PDFPDF    
Cu Filling into TSV and non-PR Sn bumping for 3 Dimension Chip Packaging
Sung-Chul Hong, Wang-Gu Lee, Jun-Kyu Park, Won-Joong Kim, Jae-Pil Jung
J Weld Join. 2011;29(1):9-13.   Published online March 4, 2011
PDFPDF    
A Study on 3-D Information Extraction using Single X-ray Image
SungMan Cho, Chun-Sam Song, Jong-hyeong Kim
J Weld Join. 2011;29(1):14-19.   Published online March 4, 2011
PDFPDF    
Warpage Study of Ultra Thin Package Used in Mobile Devices
Cha-Gyu Song, Kyoung-Ho Kim, Sung-Hoon Choa
J Weld Join. 2011;29(1):20-24.   Published online March 4, 2011
PDFPDF    
ACF COB Bonding Process using Thermosonic
Yong Song, Byung-Seung Yim, Jin-Sik Joung, Jong-Min Kim
J Weld Join. 2011;29(1):25-28.   Published online March 4, 2011
PDFPDF    
Array Lens and Pinhole-based Multi-Confocal Robot Vision System : Micro Bump Inspections in Wafer Level Packaging
MinYoung Kim, Hyun-Woo Kim, Soon-Geul Lee
J Weld Join. 2011;29(1):29-32.   Published online March 4, 2011
PDFPDF    
Parameters Study on Micro-Dispensing Deposition Write (MDDW) for High Viscous Materials
Kyung-Deok Jang, Young-Kyun Jo, Sung-Yeap Hong, Nam-Soo Kim, Tae-Eui Jeong
J Weld Join. 2011;29(1):33-35.   Published online March 4, 2011
PDFPDF    
Printable Materials and Technologies in Korea - Focused on Ink-jet and Roll to Roll (R2R)
Young-June Lee, Jeong-Hyu Lee, Nam-Soo Kim, Sung-Yeap Hong, Tae-Eui Jeong
J Weld Join. 2011;29(1):36-40.   Published online March 4, 2011
PDFPDF    
Estimation of Mechanical Properties of Sn-xAg-0.5Cu Lead-free Solder by Tensile Test
Jong-Seol Jeong, Ki-Hoon Shin, Jong-Hyeong Kim
J Weld Join. 2011;29(1):41-45.   Published online March 4, 2011
PDFPDF    
Thermo-mechanical Reliability Analysis of Copper TSV
Sung-Hoon Choa, Cha-Gyu Song
J Weld Join. 2011;29(1):46-51.   Published online March 4, 2011
PDFPDF    
Study of Metal(Au) Bump for Transverse Ultrasonic Bonding
Myeong-Gu Ji, Chun-Sam Song, Joo-Hyun Kim, Jong-Hyeong Kim
J Weld Join. 2011;29(1):52-58.   Published online March 4, 2011
PDFPDF    
A Study on Tensile Properties and HAZ Softening Depending on the Amount of Heat Input in MIG Welding of Al6082-T6
Sang-Yeob Baek, Kyung-Do Park, Won-Il Kim, Sang-Myung Cho
J Weld Join. 2011;29(1):59-64.   Published online March 4, 2011
PDFPDF    
Microstructural Characteristics of 800 ㎫ Grade High Strength Steel Weld Metals
Jaehee Lee, Sanghoon Kim, Byunghyun Yoon, Hwantae Kim, Sangcheol Kil, Changhee Lee
J Weld Join. 2011;29(1):65-73.   Published online March 4, 2011
PDFPDF    
Variation of Toughness and Porosity Formation in Weld Metal with Al Content in Self-Shielded Arc Welding Wire
Kook-soo Bang, Chan Park, Kil Woong, Woong-Seong Chang
J Weld Join. 2011;29(1):74-79.   Published online March 4, 2011
PDFPDF    
Study on the Optimization Field Welding Conditions of Low Heat-Input Pluse MIG Welding Process for 5052 Aluminum Alloy Sheets
Jae-seong Kim, Young-gi Lee, Ju-sun An, Bo-Young Lee
J Weld Join. 2011;29(1):80-84.   Published online March 4, 2011
PDFPDF    
Studies on the Improvement of Butt Welding Characteristic of Polyethylene Pipes
Ju-seon An, Kyng-won Lee, Jae-sung Kim, Bo-young Lee
J Weld Join. 2011;29(1):85-89.   Published online March 4, 2011
PDFPDF    
Al-Si Coated Boron Steel과 Zn Coated DP Steel 이종금속의 DISK Laser 용접부 미세조직과 경도
YongGyu An, ChungYun Kang, YoungSu Kim, CheolHee Kim, TaeKyo Han
J Weld Join. 2011;29(1):90-98.   Published online March 4, 2011
PDFPDF    
Improvement of Solder Joint Strength in SAC 305 Solder Ball to ENIG Substrate Using LF Hydrogen Radical Treatment
Ah-reum Lee, Seung-jae Jo, Jai-hyun Park, Chung-yun Kang
J Weld Join. 2011;29(1):99-106.   Published online March 4, 2011
PDFPDF    
Effect of B Contents on Hardness Characteristic of Disk Laser Beam Welded CP Steels
Tae-Jun Park, Jung-Woo Yu, Junil Kang, Tae-kyo Han, Kwang-Keun Chin, Chung-Yun Kang
J Weld Join. 2011;29(1):107-114.   Published online March 4, 2011
PDFPDF    
In-Process Monitoring of Micro Resistance Spot Weld Quality using Accelerometer
HeeSeok Chang, HyoChul Kwon
J Weld Join. 2011;29(1):115-122.   Published online March 4, 2011
PDFPDF    
Registration of Organizations for the Welding Personnel Education and Training based on IAB/IIW Scheme
편집부
J Weld Join. 2011;29(1):123-124.   Published online March 4, 2011
PDFPDF    
학회소식
편집부
J Weld Join. 2011;29(1):125-130.   Published online March 4, 2011
PDFPDF    
회원사 동정 외
편집부
J Weld Join. 2011;29(1):131-134.   Published online March 4, 2011
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2022 by The Korean Welding and Joining Society.

Developed in M2PI