2031545
Electrode Life Test of Resistance Spot Welding on Mg Alloy Using Dome Type Electrode
Dong-Soon Choi, In-Sung Hwan, Dong-Cheol Kim, Moon-Jin Kang
J Weld Join. 2013;31(6):27-31.   Published online January 21, 2014
PDFPDF    
Measurement of Weld Mechanical Properties of SUS316L Plate Using an Instrumented Indentation Technique
Kee-Nam Song, Sung-Deok Hong, Dong-Seong Ro
J Weld Join. 2013;31(2):37-42.   Published online June 5, 2013
PDFPDF    
A Study on Laser Weldability of Al-Si Coated 22MnB5 Steel for TWB Hot Stamping
Yong Kim, Ki-Young Park, Bo-Young Lee
J Weld Join. 2013;31(2):30-36.   Published online June 5, 2013
PDFPDF    
Recent Study of Overlay Welding on Welding methods
Ho-Cheon Yoo
J Weld Join. 2013;31(1):11-20.   Published online June 4, 2013
Evaluation of Property and Reliability of Sn3.5Ag and Sn0.7Cu Pb-free Solder Joint by Complex Vibration for Application of Automobile Electric Module
Young-Ho Ko, Jung-Hwan Bang, Jeong-Han Kim, Chang-Woo Lee
J Weld Join. 2013;31(1):6-10.   Published online June 4, 2013
2031628
A Welding Characteristics of Large Caliber-Thick Plate Pressure Vessel Low Alloy Steel (Mn-Mo)
Jong-Seok Ahn, Jin-Keun Park, Jae-Yeon Yoon
J Weld Join. 2012;30(6):10-14.   Published online December 23, 2012
PDFPDF    
2031627
Evaluation HIC Crack Resistance for Plastic Deformation of API-X65 Plate
Hoi-Soo Ryoo, Jun Seok Seo, Hee-jin Kim, Dong-Eon Lee
J Weld Join. 2012;30(6):6-9.   Published online December 23, 2012
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.

ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2022 by The Korean Welding and Joining Society.

Developed in M2PI