Development of an Inline Quality Inspection System for Resistance Spot Welds Using 3D Scanning-Based Nugget Diameter Prediction and Surface Defect Analysis
Su-Min Park, Tae-Young Kang, Seung Hoon Lee et al.
J Weld Join. 2025;43(5):581-593.   Published online October 31, 2025
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032404
A Study to Improve the Equation of Heat Input with Laser-Arc Hybrid Welding for 9% Nickel Steel
Jeong Yeol Park, Changwook Ji, Jooyoung Chun, Hyunwook Jeon
J Weld Join. 2025;43(3):252-259.   Published online June 30, 2025
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032334
Review on Ultrasonic Welding Quality Monitoring Technology
Byeong-Jin Kim, Insung Hwang, Seong-Guk Son, Chanhoon Park, Young-Min Kim
J Weld Join. 2024;42(2):215-222.   Published online April 30, 2024
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032259
Recent Research Trend of Resistance Spot Welding Quality Monitoring Technology in Korea
Young-Min Kim, Insung Hwang, Jason Cheon
J Weld Join. 2023;41(2):90-99.   Published online April 30, 2023
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032258
Recent Research Trend of Arc Welding Quality Monitoring Technology in Korea
Young-Min Kim, Jason Cheon
J Weld Join. 2023;41(2):81-89.   Published online April 30, 2023
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Prediction of Indentation Depth of Resistance Spot Welding Using Electrode Displacement Signal
Sehyeon Kim, Insung Hwang, Munjin Kang, Jiyong Park, Jiyoung Yu
J Weld Join. 2021;39(3):314-322.   Published online June 11, 2021
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Evaluation of Welding Quality using Servo-Gun Displacement Data for Field Spot Welding
Jaesung Kim, Jooheon Park, Sanghyeok Jeong, Bokdeok Seo
J Weld Join. 2020;38(5):460-468.   Published online October 26, 2020
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Development of Quality Inspection System for Fillet Welding Based on Laser Vision Sensor
Ui-Tae Jeong, Hyeong-Jun Lee, In-Soo Lee
J Weld Join. 2018;36(6):52-59.   Published online December 5, 2018
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
A Study on Real-time Prediction of Bead Width on GMA Welding
Joon-Sik Son, Ill-Soo Kim, Hak-Hyoung Kim
J Weld Join. 2007;25(5):64-70.   Published online January 28, 2008
PDFPDF    
A Study on Monitoring for Process Parameters Using Isotherm Radii
Ill-Soo Kim, Kwang-Suk Chon, Joon-Sik Son, Joo-Hwan Seo, Hak-Hyoung Kim, Ji-Yeon Shim
J Weld Join. 2006;24(5):37-42.   Published online January 4, 2007
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2026 by The Korean Welding and Joining Society.

Developed in M2PI