Study on Real-Time Porosity Defect Detection Through Neural Network Structure Optimization using Genetic Algorithm in GMAW
Dongwook Lee, Chengnan Jin, Sehun Rhee
J Weld Join. 2021;39(5):542-551.   Published online September 17, 2021
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Optimization of Laser Welding Parameters in Titanium Sheet Using Grey-Fuzzy Logic
Byeong-Ju Jin, Min-Ho Park, Tae-Jong Yun et al.
J Weld Join. 2017;35(6):59-66.   Published online November 16, 2017
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Laser Welding of Automotive Transmission Components
Young-Nam Ahn, Cheolhee Kim
J Weld Join. 2011;29(6):45-48.   Published online January 20, 2012
PDFPDF    
Study on the Optimization of Pulse GTAW Process for Diaphragm with Thin Thickness
Hyoung-Jin Park, In-Sung Hwang, Munjin Kang, Sehun Rhee
J Weld Join. 2008;26(1):63-68.   Published online March 21, 2008
PDFPDF    
Optimization of Process Parameters Using a Genetic Algorithm for Process Automation in Aluminum Laser Welding with Filler Wire
YoungWhan Park
J Weld Join. 2006;24(5):67-73.   Published online January 4, 2007
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI