Determination of Optimal Conditions for a Gas Metal Arc Welding Process Using Genetic Algorithm
김동철, 이세헌

Correspondence:   Published online October 25, 2000
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
985
View
0
Download
Related articles
Spectrogram Based Detection Algorithm for Back-Bead in Gas Metal Arc Welding Process using Convolution Neural Network  2021 April;39(2)
Determination of Optimal Weld Parameter for Joining Titanium Alloys by Gas Tungsten Arc Welding using Taguchi Method  2021 February;39(1)
A Study on Optimization of Fillet in Laser Welding Process for 9% Ni Steel Using Gradient-Based Optimization Algorithm  2020 October;38(5)
Study on a Residual Stress Reduce in Laser Welding Process using Ti6Al4V  2016 December;34(6)
A Study on Bead Geometry Prediction the GMA Fillet Welding using Genetic Algorithm  2012 December;30(6)
Spectrogram Based Detection Algorithm for Back-Bead in Gas Metal Arc Welding Process using Convolution Neural Network  2021 April;39(2)
Determination of Optimal Weld Parameter for Joining Titanium Alloys by Gas Tungsten Arc Welding using Taguchi Method  2021 February;39(1)
A Study on Optimization of Fillet in Laser Welding Process for 9% Ni Steel Using Gradient-Based Optimization Algorithm  2020 October;38(5)
Study on a Residual Stress Reduce in Laser Welding Process using Ti6Al4V  2016 December;34(6)
A Study on Bead Geometry Prediction the GMA Fillet Welding using Genetic Algorithm  2012 December;30(6)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.           Developed in M2PI