Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2023-03.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Recent Trends in the Manufacture of Composites by Friction Stir Processing

J Weld Join > Volume 30(5); 2012 > Article
Journal of KWJS 2012;30(5):16-21.
DOI: https://doi.org/10.5781/KWJS.2012.30.5.16    Published online November 30, 2012.
Recent Trends in the Manufacture of Composites by Friction Stir Processing
Yong-Ha Jeong, Sung-Tae Hong, Ho-Chul Seo
Abstract
  In various manufacturing industries including automotive industries, the use of lightweight materials is rapidly increasing. In the use of lightweight materials, it is obvious that enhancing their mechanical or material properties without significant weight increase is extremely beneficial. One method to enhance material properties of a lightweight material while maintaining its light weight is fabricating metal matrix composites (MMC) by adding reinforcements to the material. In the present study, recent trends in the manufacture of MMC by friction stir processing are briefly reviewed.
Key Words: Lightweight materials, Metal matrix composites, Friction stir processing


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2023 by The Korean Welding and Joining Society.

Developed in M2PI