Laser Welding of Seal Tube for Instrumented Irradiation Fuel Test
Soo-Sung Kim, Chul-Yong Lee, Woong-Ki Kim, Geun-Il Park, Jinh-Yun Koh, Jun-Seok Seo





Correspondence:   Published online January 26, 2006
ABSTRACT
This work was carried out to obtain sound welds and to select a most suitable binary metal joint among three different dissimilar binary metal combinations such as Zr-4/Ta, Mo/Ta and Ti/Ta(seal tube/sensor sheath) joints for the instrumented nuclear fuel irradiation test. To do this, Taguchi experimental method was employed to optimize the experimental data. In addition, metallography, micro-focus x-ray radiography and hardness test were conducted to examine the welds. From the weld bead appearance, penetration depth and bead width as well as weld defects standpoint, Zr-4/Ta joint is suggested for the circumferential joining between a seal tube and a sensor sheath. The optimized welding parameters based on Zr-4/Ta joint are suggested as well.
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,165
View
0
Download
Related articles
Laser Soldering Properties of MEMS Probe for Semiconductor Water Testing  2021 August;39(4)
Laser Welding of Automotive Transmission Components  2011 December;29(6)
Laser Beam Welding Technology of Seal Tube for Radiation-Resistant LVDT Manufacturing  2011 October;29(5)
Technology of the End Cap Laser Welding for Irradiation Fuel Rods  2003 October;21(6)
Arc and Laser Welding of Al Alloys for the Transportation Applications   2001 April;19(2)
Laser Soldering Properties of MEMS Probe for Semiconductor Water Testing  2021 August;39(4)
Laser Welding of Automotive Transmission Components  2011 December;29(6)
Laser Beam Welding Technology of Seal Tube for Radiation-Resistant LVDT Manufacturing  2011 October;29(5)
Technology of the End Cap Laser Welding for Irradiation Fuel Rods  2003 October;21(6)
Arc and Laser Welding of Al Alloys for the Transportation Applications   2001 April;19(2)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society.           Developed in M2PI