Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-05.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 A Study on the Formation Mechanism of Discontinuities in Co2 Laser Fusion Zone of Fe-Co-Ni Sintered Segment and Carbon Steed

Journal of KWJS 2003;21(3):58-67.
Published online June 25, 2003.
Fe-Co-Ni 분말 소결 금속과 탄소강의 이종재료간 레이저 용접부의 결함형성기구 연구
, , ,
 
A Study on the Formation Mechanism of Discontinuities in Co2 Laser Fusion Zone of Fe-Co-Ni Sintered Segment and Carbon Steed
신민효, 김태웅, 박희동, 이창희