Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-05.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Analysis on The Three-Dimensional Unstationary Heat Conduction on The Welding of Thick Plate by F. E. M.

Journal of KWJS 1991;9(2):37-43.
Published online June 25, 1991.
유한요소법에 의한 후판용접시의 3차원 비정상열전도해석
,
 
Analysis on The Three-Dimensional Unstationary Heat Conduction on The Welding of Thick Plate by F. E. M.
방한서, 김유철