Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 A Study on the Fatigue Crack Growth Behavior of Aluminum Alloy Weldments in Welding Residual Stress Fields

Journal of KWJS 1989;7(1):28-35.
Published online March 27, 1989.
용접 잔류응력장 중에서의 Aluminum-Alloy 용접재의 피로균열성장거동 연구
,
 
A Study on the Fatigue Crack Growth Behavior of Aluminum Alloy Weldments in Welding Residual Stress Fields
최용식, 정영석