Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2025-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 100 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 101 Evaluation of HIC/SSCC Resistance for API-X70 Pipe Manufactured by JCO Bending Process and SA Welding

J Weld Join > Volume 32(5); 2014 > Article
Journal of Welding and Joining 2014;32(5):431-436.
DOI: https://doi.org/10.5781/JWJ.2014.32.5.1    Published online October 30, 2014.
Evaluation of HIC/SSCC Resistance for API-X70 Pipe Manufactured by JCO Bending Process and SA Welding
Hoi-Soo Ryoo*, Hee Jin Kim*, Dong-Eon Lee**
Correspondence:  Hoi-Soo Ryoo,
Email: hsryoo@kitech.re.kr
Abstract
This study aims at manufacturing SA welded API-X70 line-pipe with sour gas resistance. A pipe was manufactured by JCO bending process and SA welding using the API-X70 plate guaranteed HIC resistance. SA welded pipe was expanded in order to reduce the residual stress. The evaluation of a pipe for resistance to HIC and SSCC were performed by the RS D 0004 and RS D 0005 standards. For verification that a pipe has acceptable resistance to HIC, fullscale test was carried out. Results showed no cracking for the HIC and SSCC.
Key Words: API-X70, JCO(J-ring, C-ring, O-ring) bending, SAW(submerged arc welding), HIC(hydrogen induced cracking), SSCC(sulfide stress corrosion cracking), Fullscale HIC test


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2025 by The Korean Welding and Joining Society.

Developed in M2PI