Journal of KWJS 2011;29(4):67-72.
Published online September 12, 2011.
십자형 필릿 용접부에서의 피로파괴 형상과 특성
, ,
 
Patterns and Characteristics of Fatigue Failure in Cruciform Fillet Weld Joint
Yong-Bok Lee, Joon-Ki Chung, Sang-Heup Park
Abstract
  The proportion of the welding in the production process of machinery, buildings and marine structures is increasing and the joining are mainly conducted by butt and fillet weld. In the case of fillet weld, the shape of structures is complicated depending on the constraint on the geometry of the structures, therefore, the full penetration is mostly difficult. Accordingly, it is necessary to establish safe and economical criteria of design of the structures through the strength based on the penetration state of the fillet weld. Patterns of fatigue failure in cruciform fillet weld jont appear in the form of the root, toe and mixed failure. In the case of toe and mixed failure, the fatigue strength is higher than root failure. Therefore, we have to make the enough depth of penetration or perform the welding work through improving the fatigue strength of cruciform joints in welded structures. So it is necessary to optimize the penetrated depth in the range of the possible mixed failure and find the way in the cost-effective design to lessen the amount of the welding work.
Key Words: Fillet weld, Fatigue failure, Fatigue strength, Penetrated depth, Toe failure, Root failure, Mixed failure


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2026 by The Korean Welding and Joining Society.

Developed in M2PI