Journal of KWJS. 1993;11(1):42-51. Published online March 25, 1993.
- A Study on the Dynamic Fracture Toughness of Welding Structural Steels by Instrumented Impact Testing ( A Study on the brittle zone of welding heat affected )
-
김헌주, 김경민, 윤의박
-