ABOUT
Aims and scope
About the journal
Editorial board
Copyright and open access
Best practice
BROWSE ARTICLES
Current issue
All issues
Ahead-of print
Most view
Most cited
ARTICLE CATEGORY
Research Paper
Review Paper
Technical report
Technical review
Special Issue
Erratum
FOR CONTRIBUTORS
Publish with
JWJ
Ethical guidelines
Open access
Instructions for authors
Instructions for peer reviewers
Readers
Copyright transfer agreement
E-submission
Search
Close
Previous issues
Volume 6 Issue 3
기계 , 구조물용 세라믹과 금속과의 접합가공 기술
김영식
Journal of KWJS. 1988;6(3):1-7.
Flux Cored wire의 특성 및 사용상의 유의점
김경중
Journal of KWJS. 1988;6(3):8-20.
Behavior of Angular Distortion in Butt Joint Welding of Thin Plate Structure
배강열, 김희진
Journal of KWJS. 1988;6(3):21-26.
Effect of Chemical Compositions on the Weldablity of Quenched and Tempered High Strength Steels
장웅성, 김숙환, 장래웅, 엄기원
Journal of KWJS. 1988;6(3):27-36.
A Study on the Residual Stress Measurement by Hole Drilling Method using Air-abrasive Jet Machine ( I )
이택순, 최병길, 전상윤
Journal of KWJS. 1988;6(3):37-42.
Effects of KII on Fatigue Crack Propagation Behavior of Weldzone in Generally Rolled Steel for Marine Structure
한문식, 김상철
Journal of KWJS. 1988;6(3):43-55.