Journal of KWJS 2012 April;30(2) :70-75.
Published online May 16, 2012.
doi:https://doi.org/10.5781/KWJS.2012.30.2.70
Effect of Nitrogen Volume in Ar-N2 Shielding Gas on Microstructure and Hardness of GTA Welded Pure Ti
Hyun-Jun An, Ae-Jeong Jeon, Jae-Keun Hong, Bo-Young Jeong, Jong-Sub Lee, Chung-Yun Kang





Correspondence:   Published online May 16, 2012
ABSTRACT
  In this study, effect of nitrogen volume in the shielding gas of Ar-N₂ mixing gas on the bead shape, hardness and microstructure of GTA welds of 3mm thick Commercial Pure Ti was investigated. As the nitrogen volume increased, the welding current for full penetration was reduced and hardness in the fusion zone significantly increased compared with that of the base metal, but there is no difference in the hardness of HAZ. Microstructure in the fusion zone with pure Ar gas changed from equiaxed alpha of the base metal to serrated alpha. On the other hand, microstructure using Ar-N₂ mixing gas changed to acicular alpha. With the increasing of nitrogen content, the amount of acicular alpha increased and the size of that was fine.
Keywords: CP Ti;GTAW;Shielding gas;Ar-N₂ mixing gas;Microstructure;Hardness
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
976
View
0
Download
Related articles
Effect of Tensile Properties and Microstructure on the Heat Input of Ni-Doped High Manganese Welding Wire  2018 February;36(1)
Recent Advances in Friction-stir Welding Process and Microstructural Investigation of Friction Stir Welded Pure Titanium   2017 August;35(4)
Effect of Heating Rates on Microstructures in Brazing Joints of STS304 Compact Heat Exchanger using MBF 20  2016 April;34(2)
Effect of Hot-stamping on Microstructures and Tensile Properties of Al-Si Coated Boron Steel Welds with Laser Source  2013 December;31(6)
Effects of Oxygen Contents in Shielding Gas on the Properties of Ferritic Stainless Steel GTA Weld  2010 October;28(5)
Effect of Tensile Properties and Microstructure on the Heat Input of Ni-Doped High Manganese Welding Wire  2018 February;36(1)
Recent Advances in Friction-stir Welding Process and Microstructural Investigation of Friction Stir Welded Pure Titanium   2017 August;35(4)
Effect of Heating Rates on Microstructures in Brazing Joints of STS304 Compact Heat Exchanger using MBF 20  2016 April;34(2)
Effect of Hot-stamping on Microstructures and Tensile Properties of Al-Si Coated Boron Steel Welds with Laser Source  2013 December;31(6)
Effects of Oxygen Contents in Shielding Gas on the Properties of Ferritic Stainless Steel GTA Weld  2010 October;28(5)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.