Research Paper
-
Research Papers
Review on Ultrasonic Welding Quality Monitoring Technology
- Byeong-Jin Kim, Insung Hwang, Seong-Guk Son, Chanhoon Park, Young-Min Kim
- J Weld Join. 2024;42(2):215-222.
-
Research Papers
Mechanical Properties of Fe-TiC Composites for Friction Stir Welding Tool Application by a Spark Plasma Sintering
- Bum-Soon Park, Min-Hyeok Yang, Hyun-Kuk Park
- J Weld Join. 2024;42(2):206-214.
-
Research Papers
Effect of Cr on the Hot Ductility of Austenitic Fe-Mn-Al-C Lightweight Steel
- Seonghoon Jeong, Joonoh Moon, Seong-Jun Park, Changhee Lee
- J Weld Join. 2024;42(2):200-205.
-
Research Papers
A Study on the Microstructure and Mechanical Properties of Electron Beam Welds of SA508 Gr.3 Cl.1 steel with Different Heat Treatment conditions for Small Modular Reactor
- In-Chul Jung, Heon-Min Suh, In-Sung Choi, Jeong Suh, Seong-Woo Jo, Deog-Nam Shim, Hyun-Uk Hong
- J Weld Join. 2024;42(2):193-199.
-
Research Papers
High-Speed Thermo-Compression Sinter-Bonding Properties in Air of a Paste Containing Dendritic Cu Particles Having Oxalate Skins
- Horyun Kim, Jong-Hyun Lee
- J Weld Join. 2024;42(2):184-192.
-
Research Papers
Thermal Cycling Performance of Heterogeneous Solder Ball Joints with Sn-3.0Ag-0.5Cu and Sn-0.75Cu(-Ni,Bi) Solder Ball Composition for BGA Package
- Joo Young Bae, Mi-Song Kim, So-Hee Hyun, Jong-Hyun Lee, Jeong Tak Moon, Young-Woo Lee, Seul Gi Lee, Hyeong-Tea Kim, Seung-Kwan Baek, Won Sik Hong
- J Weld Join. 2024;42(2):174-183.
-
Research Papers
Optimization of TLPS Bonding Process and Joint Property using Ni-Sn Paste for High Temperature Power Module Applications
- Da-Gyeong Han, Dong-Hwan Lee, Jeong-Won Yoon
- J Weld Join. 2024;42(2):165-173.
-
Research Papers
Recent Progress of TGV Technology for High Performance Semiconductor Packaging
- Beom Chang Seok, Jae Pil Jung
- J Weld Join. 2024;42(2):155-164.
-
Research Papers
Mechanical Bonding Properties of Solderable Anisotropic Polymer Composite containing Low-Melting-Point and High-Melting-Point Solder Fillers
- Yi Hyeon Ha, Myeong Jin Jung, Jong-Moon Park, Sung Woo Choi, Jong-Min Kim, Byung-Seung Yim
- J Weld Join. 2024;42(2):149-154.
-
Research Papers
Prediction of Laser Welding Distortion in Cylindrical Shell Structures Using Direct Application of Inherent Strain
- Ji-Hong Yoon, Young-Soo Yang, Sung-Hoon Kim, Se Hwan Lee, Jeong-Ung Park
- J Weld Join. 2024;42(1):134-140.
-
Research Papers
A Study on the Establishment of Alternative Verification Standard of Ballistic Ttest for Armored Steel Arc Welding Procedure
- Yong Kim, Min Chul Oh, Ji Young Jang, Do Hui Kim
- J Weld Join. 2024;42(1):125-133.
-
Research Papers
Development of Creep and Mechanical Properties for SMAW Cr-Mo-X Steel Welds
- Sanghyun Bae, Yongchul Kim, Stephen Liu
- J Weld Join. 2024;42(1):117-124.
-
Research Papers
A Study on the Weldability of Cylindrical Secondary Battery Material using Green Laser
- Hyun Jong Yoo, Jun Su Park, Ik Geun Jeon, Myung Jin Kim, Jong Sik Kim, Hee Shin Kang
- J Weld Join. 2024;42(1):106-116.
-
Research Papers
Non-Destructive Testing of Laser Welded Hydrogen Storage Tank Liner Using Optical Coherence Tomography
- Ryoonhan Kim, Dongsig Shin, Sujin Lee, Danbi Song, Sang-Eon Park, Wooyoung Chung, Sangbae Han
- J Weld Join. 2024;42(1):99-105.
-
Research Papers
Research Trends in the Directed Energy Deposition Method of Heterogeneous Materials
- Raj Narayan Hajra, Jeoung Han Kim
- J Weld Join. 2024;42(1):88-98.
-
Research Papers
Assessment of Ttensile-Shear and T-Peel Strengths for Cu-STS 304 Dissimilar Overlap Welded Joints using Single-Mode Fiber Laser with High Welding Speeds
- Youngjin Eun, Sanghoon Kang, Minjung Kang
- J Weld Join. 2024;42(1):81-87.
-
Research Papers
Review on Laser Welding Technology on Aluminum and Copper Dissimilar Materials for Secondary Batteries Assembly
- Jaewoo Cho, Taehyun Lee, Heeseon Bang, Soongkeun Hyun, Cheolhee Kim
- J Weld Join. 2024;42(1):69-80.
-
Research Papers
A Study on Mechanical/Metallurgical Characteristic of Welded Joints According to Heat Input and Gap in Al/Cu Laser Welding
- Chan Yang Lee, Min Chul Oh
- J Weld Join. 2024;42(1):62-68.
-
Research Papers
Machine Learning Algorithm Comparison for the Performance Evaluation of Manual Welding Process
- Chang Sub Song, Jong-Ho Nam
- J Weld Join. 2024;42(1):50-61.
-
Research Papers
Improving the Accuracy of Predicting the Shaft Part Thermal Deformation of an LNG Fuel Powered Container Ship Based on the Inherent Strain
- Jun-Seok Park, Jung-Goo Park, Jung-Kwan Seo
- J Weld Join. 2024;42(1):41-49.
-
Research Papers
A Study on the Residual Stress of Seam Pipe Cutting and Girth Welding
- Ji-Sun Roh, Myung-Su Yi, Jung-Goo Park, Myung-Hyun Kim
- J Weld Join. 2024;42(1):27-40.
-
Research Papers
A Study on Deformation due to Steel Constraint during Butt Welding and Line Heating of Thick-Plate in FLNG Topside Bearing Node
- Dong-Hee Park, Jung-Goo Park, Jae-Myung Lee
- J Weld Join. 2024;42(1):18-26.
-
Research Papers
Review the Ultimate Strength According to Welding Deformation Criteria of Thin Plates Under In-plane Compression
- Myung-Su Yi, Joo-Shin Park
- J Weld Join. 2024;42(1):9-17.
-
Research Papers
Investigation on the Microstructure Evolution and Mechanical Properties of High Carbon Steel Friction Welded Joint
- Kyoung-Hwan Kim, Bongjun Kim, Joonoh Moon, Jungwon Lee, Yonghyun Kim
- J Weld Join. 2023;41(6):566-572.
-
Research Papers
Bonding Characteristics of Solder and Sinter Joints on Active-Metal-Brazing Substrates with Nano Sputtered Ag-Cu-Ti Brazing Filler Metal
- Mi-Song Kim, Won Sik Hong, Yong-Mo Kim
- J Weld Join. 2023;41(6):558-565.
-
Research Papers
Review on Recent Laser Welding Trend in Electric Powered Vehicle Production
- Hae Woon Choi
- J Weld Join. 2023;41(6):548-557.
-
Research Papers
Effect of Assistant Gas Pressure on Cutting Performance when 80mmt Stainless Steel Laser Cutting in Pressurized Underwater Environment
- Jaeook Jeon, Moo-Keun Song, Kwan Kim, Sujin Lee, Dae-won Cho, Dongsig Shin, Jongdo Kim
- J Weld Join. 2023;41(6):540-547.
-
Research Papers
Study on the Comparison of Electron Beam Welding and Hybrid Laser-Arc Welding of Thick High-Manganese Steel Plate for Cryogenic Applications
- Insung Choi, Heon min Seo, In-Chul Jung, Kwang-Hyeon Lee, Jeong Suh
- J Weld Join. 2023;41(6):528-539.
-
Research Papers
Electrochemical Metallic Ion Migration Property of Multi-Layer Ceramic Capacitor for Car Electronics
- Won Sik Hong, Mi-Song Kim, Joo Young Bae, So-Hee Hyun, Heehun Bae, Joon-Seok Kyeong, Eun-Jeong Park, Jongeul Kim, Ju-Seok Oh
- J Weld Join. 2023;41(6):519-527.
-
Research Papers
A Study on Deformation According to Steel Constraints During Thick-Plate Fillet Welding and Line Heating
- Dong-Hee Park, Jung-Goo Park, Chang-Woo Park, Jin-Hyuk Yang, Jun-Seok Park, Ji-Sun Roh, Myung-Su Yi, Do-Kyun Kim, Jae-Myung Lee
- J Weld Join. 2023;41(6):508-518.
-
Research Papers
A Study on Bead on Plate (BOP) Test for Laser Welding Application of Stainless Steel to Liquified Hydrogen Tank (PART I: STS 304)
- Eul-Yong Ha, Chang-Min Pyo, Young-Hyun Kim, Jin-Seok Woo, Sun-Pil Kim, Myung-Su Yi, Sung-Wook Kang, Chang-Wook Ji, Jae-Woong Kim
- J Weld Join. 2023;41(6):500-507.
-
Research Papers
Comparative Analysis of SPR and SPR-Bonded Joints of Hot Press Forming Steel and AA5052 under Corrosive Conditions
- Han-ju Lee, Savyasachi Nellikode, Tae-Young Kang, Yeong-Do Park
- J Weld Join. 2023;41(6):486-499.
-
Research Papers
Effect of Carburization on the Microstructure and Laser Weldability of 316L Stainless Steel
- Gitae Park, Mokyoung Lee, Chan Kyu Kim, Sangwoo Song, Sung Chul Cha, Heon Joon Park, Jun-Ho Kim, Boyoung Jeong
- J Weld Join. 2023;41(6):475-485.
-
Research Papers
Review on Ultrasonic and Laser Welding Technologies of Multi-Layer Thin Foils for the Lithium-Ion Pouch Cell Manufacturing
- Musung Kim, Heeseon Bang, Soongkeun Hyun, Sung Yi, Cheolhee Kim
- J Weld Join. 2023;41(6):462-474.
-
Research Papers
Effect of Welding Process on Microstructure and Impact Toughness of Welds in High Nitrogen TiN Steel
- Soon-Doo Kwon, Sang-Hoon Jeong
- J Weld Join. 2023;41(6):454-461.
-
Research Papers
Market and Development Trends in Thermal Cutting Technology for Nuclear Power Plant Decommissioning
- Sujin Lee, Jongdo Kim, Jeong Suh, Dongsig Shin, Induck Park
- J Weld Join. 2023;41(6):440-453.
-
Research Papers
A Study on the Microstructure and Mechanical Properties of SA508 Gr.3 Cl.1 Steel Cladded by a Laser Beam using Alloy 82 and 308L Powders for Small Modular Reactor
- In-Chul Jung, Insung Choi, Kwang-Hyun Lee, Jeong Suh, Seong-Woo Jo, Shi-Hong Kim, Hyun-Uk Hong
- J Weld Join. 2023;41(6):429-439.
-
Research Papers
Consideration on the Applicability of Electron Beam Welding for the Manufacture of Small Modular Reactor
- In-Chul Jung, Jeong Suh
- J Weld Join. 2023;41(6):422-428.
-
Research Papers
Review on High-Energy Beam Based Processing Technologies for Fabrication of Small Modular Reactor
- Insung Choi, Jeong Suh, In-Duck Park, Kwang-Hyeon Lee, In-Chul Jung
- J Weld Join. 2023;41(6):411-421.
-
Research Papers
A Study on the Characteristics about Shaft Deflection According to the Change in Manufacturing Sequences
- Jun-Seok Park, Joo-Shin Park, Jung-Kwan Seo
- J Weld Join. 2023;41(5):396-402.
-
Research Papers
Bonding Property of Flip-Chip Chip-Scale Package with Vacuum Reflow and Thermal Compression Bonding Processes
- So-Hee Hyun, Hye Min Lee, Mi-Song Kim, Won Sik Hong
- J Weld Join. 2023;41(5):387-395.
-
Research Papers
Bonding Property of Middle Temperature Sn-Ag-Cu Solder Ball Joint of Ball Grid Array Package
- Joo Young Bae, Mi-Song Kim, Hye Min Lee, Seul Gi Lee, Young-Woo Lee, Jeong Tak Moon, Won Sik Hong
- J Weld Join. 2023;41(5):379-386.
-
Research Papers
Hot Cracking Characteristics During Single-Mode Fiber and Green Laser Welding Processes in Lithium-Ion Battery Pack Manufacturing
- Jae-Hyeon Park, Myung-Jin Kim, Heeshin Kang, Wonah Park, Eun-Joon Chun
- J Weld Join. 2023;41(5):367-378.
-
Research Papers
A Review on Effects of Weld Porosity in Laser-Arc Hybrid Welding for Aluminum Alloys
- Seong hyun Kim, Jae-Deuk Kim, Hyun-Uk Jun, Joo Yong Cheon, Seungjong Yun, Yangdo Kim, Changwook Ji
- J Weld Join. 2023;41(5):358-366.
-
Research Papers
Prediction Model for Tensile Shear Strength of Gas Metal Arc Weld using a Laser Vision Sensor
- Changhoon Lee, Dong-Yoon Kim, Jason Cheon, Jiyoung Yu
- J Weld Join. 2023;41(5):349-357.
-
Research Papers
Effects of Welding Parameters on Droplet Transfer and Bead Geometry in Laser Welding with Aluminum and Stainless Steel Filler Wires
- Joonghyeon Shin, Seung Hwan Lee, Minjung Kang
- J Weld Join. 2023;41(5):342-348.
-
Research Papers
A Study on Gap Bridging Formation Conditions in Butt Root Pass Welding Using GTAW
- Daekyu Park, Changsub Song, Youngwhan Park
- J Weld Join. 2023;41(5):335-341.
-
Research Papers
Strength Evaluation of Welded Aluminum T-joints, as a Function of Its Welding Process, Execution, Filler Material, and Weld Root Penetration
- Johannes Gaigl
- J Weld Join. 2023;41(5):327-334.
-
Research Papers
Understanding the Effects of Surface Finish on Diffusion Bonding of AZ31 Alloys
- Matthew Criado, Abhijit Roy, John Ohodnicki, Nicholas Tondravi, Hannah Fischer, Alejandro Almarza, Howard A. Kuhn, Prashant N. Kumta
- J Weld Join. 2023;41(5):317-326.
-
Research Papers
Development of an Arc Image Classification Algorithm in Tip-Rotating Arc Welding using Camera Image Monitoring and Deep Learning
- Sol Mi Lee, Young Whan Park
- J Weld Join. 2023;41(4):299-307.