ABSTRACT
  Spot welding which use the main process for side block production of stainless steel railway vehicle is legged behind in laser welding about a quality and productivity. Although the laser welding has many potential advantages such as low heat input and aspect ratio of weld bead, its application to a new structural component still is required many engineering data including mechanical properties such as tensile, fatigue strength, etc on. Therefore, experimental analysis was carried out to understand the fatigue phenomena of different thickness stainless steel overlap joining panels by Nd:YAG laser welding. The fatigue life curves were obtained through fatigue tests with the various levels of applied load. The fatigue life is related with the parameters such as gap size and penetration depth through experiment. As the results, tensile strength and fatigue life were proportional in heat input level and gap was identified the major factor for fatigue life. Also we could know that deferent δ-ferrite content at HAZ depend on welding heat input was important factor to determine a formation of initial crack and total fatigue life cycle.
Keywords: Stainless Steel;Laser Welding;Fatigue life;Overlap Joining;Railway Vehicle;δ-ferrite
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
912
View
0
Download
Related articles
Influence of Gas Metal Arc Welding Parameters on the Bead Properties in Automatic Cladding   2017 February;35(1)
The Effect of Alloying Elements on Weldability and Corrosion Resistance of Austenitic Stainless Steels(I)  2012 June;30(3)
Effects of Oxygen Contents in Shielding Gas on the Properties of Ferritic Stainless Steel GTA Weld  2010 October;28(5)
Effects of Welding Parameters on Weld Metal Strength and Recovery of Alloying Elements in FCAW  2008 April;26(2)
The Effects of Welding Parameters on the Weld Shape in Pulsed GTA Welding of a STS304L Stainless Steel Capsule  2007 October;25(5)
Influence of Gas Metal Arc Welding Parameters on the Bead Properties in Automatic Cladding   2017 February;35(1)
The Effect of Alloying Elements on Weldability and Corrosion Resistance of Austenitic Stainless Steels(I)  2012 June;30(3)
Effects of Oxygen Contents in Shielding Gas on the Properties of Ferritic Stainless Steel GTA Weld  2010 October;28(5)
Effects of Welding Parameters on Weld Metal Strength and Recovery of Alloying Elements in FCAW  2008 April;26(2)
The Effects of Welding Parameters on the Weld Shape in Pulsed GTA Welding of a STS304L Stainless Steel Capsule  2007 October;25(5)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.