Finite Element Analysis of the Stress Concentrations for Butt Welded Joints |
Byeong-Choon Goo, Byung-Il Choi, Jai-Hoon Kim |
|
Correspondence:
Published online September 15, 2004
|
|
|
The purpose of this study is to investigate the intluence of weld bead profiles on stress concentration factors of double V groove butt-welded joints. The intluence of three parameters such as toe radii, tlank angles and bead heights on the stress concentration factors is studied by finite element analysis. It is shown that the three parameters have similar effects on the stress concentration factors. Finally a formula to estimate the stress concentration factors considering the three parameters and others is proposed and estimated results are compared with the results obtained by finite element analysis. |
|
|
|
|
 |
|
|
 |
Register for e-submission |
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
|
Manuscript Submission |
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
|
Free archive |
Anyone may access any past or current articles without logging in.
|
|
|