Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Fatigue Strength Evaluation on the IB-Type Spot-welded Lap Joint of 304 Stainless Steel Part 2 : Strain Energy Density

Journal of KWJS 1999;17(6):32-37.
Published online December 27, 1999.
304 스테인리스 박강판 IB형 점용접이음재의 피로강도 평가 Part 2 : 변형에너지밀도에 의한 평가
, ,
 
Fatigue Strength Evaluation on the IB-Type Spot-welded Lap Joint of 304 Stainless Steel Part 2 : Strain Energy Density
손일선, 오세빈, 배동호