ABSTRACT
  GMA welding process is a production process to improve productivity for the provision of higher welding quality of material. These includes numerous process variables that could affect welding quality, productivity and cost savings. Recently, the welding part of construction equipment had frequent failure of major components in the welding part of each subsidiary material due to shock which is very poor according to the welding part. Therefore, the implementation of sound welding procedure is the most decisive factor for the reliability of construction machinery. The data generated through experiments conducted in this study has validated its effectiveness for the optimization of bead geometry and process variables is presented. The criteria to control the process parameters, to achieve a good bead geometry. This study has developed mathematical models and algorithms to predict or control the bead geometry in GMA fillet welding process.
Keywords: Fillet welding;Taguchi method;Mathematical model;Sensitivity analysis
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,246
View
0
Download
Related articles
An Experiment Study for S/N Ratio of Bead Geometry for Guaranteeing the Welding Quality in Bellows Weld Joint  2017 April;35(2)
An Experiment Study for Hardness Characteristic of Weldment according to Welding Heat-Input of Vertical GMA Welding Process  2017 April;35(2)
Experimental Study on Evaluation of Bonding Strength of Adhesively Bonded Joints by Adhesive  2012 December;30(6)
A Experiment Study of Torch Distance on Automated Tandem GMA Welding System  2012 December;30(6)
A Experiment Study on Selection the Optimal Condition for GMA Root-pass Welding in Overhead and Vertical Position  2012 December;30(6)
An Experiment Study for S/N Ratio of Bead Geometry for Guaranteeing the Welding Quality in Bellows Weld Joint  2017 April;35(2)
An Experiment Study for Hardness Characteristic of Weldment according to Welding Heat-Input of Vertical GMA Welding Process  2017 April;35(2)
Experimental Study on Evaluation of Bonding Strength of Adhesively Bonded Joints by Adhesive  2012 December;30(6)
A Experiment Study of Torch Distance on Automated Tandem GMA Welding System  2012 December;30(6)
A Experiment Study on Selection the Optimal Condition for GMA Root-pass Welding in Overhead and Vertical Position  2012 December;30(6)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.