Experimental Study on Evaluation of Bonding Strength of Adhesively Bonded Joints by Adhesive
Ki-Yeob Kang*, Jae-Myung Lee*
*Dept. of Naval Architecture and Ocean Engineering, Pusan National University, Busan 609-735, Korea
Correspondence: Jae-Myung Lee  Email: jaemlee@pusan.ac.kr
  Published online December 23, 2012
ABSTRACT
In this study, the bonding strengths of adhesively bonded joints are experimentally investigated. A series of lap-shear tests are conducted using single lap type adhesive joints. In order to analyse the joint fabrication factors that affected the bonding strength, the parametric tests are conducted with various thickness of adhesive, surface roughness and fillet of adhesive. In addition, for the comparative study with the welded joint, lap-shear tests using specimens with 2 welded sides and 4 welded sides are also carried out. The quantitative results of the strength analysis are summarized, and some proposals are made on setting up testing standards for adhesively bonded joints.
Keywords: Lap shear joint | Adhesive thickness | Surface roughness of adherends | Tensile-shear strength
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
2,284
View
7
Download
Related articles
A Study on the Evaluation of Fatigue Strength of Welded Lap Joint with Element Stress Approach  2014 February;32(1)
Evaluation of Failure Mode and Strength on Baking Time of Adhesive for Hybrid Joining  2011 December;29(6)
A Experiment Study for Selection of Welding Condition of fillet Welded Structure  2011 August;29(4)
Strength Evaluation of Adhesively Bonded Single-Lap Joints by Ultrasonic Signal Analysis   2004 October;22(5)
Evaluation of Flaws in Adhesively Bonded Joint using Ultrasonic Signal Analysis  2004 April;22(2)
A Study on the Evaluation of Fatigue Strength of Welded Lap Joint with Element Stress Approach  2014 February;32(1)
Evaluation of Failure Mode and Strength on Baking Time of Adhesive for Hybrid Joining  2011 December;29(6)
A Experiment Study for Selection of Welding Condition of fillet Welded Structure  2011 August;29(4)
Strength Evaluation of Adhesively Bonded Single-Lap Joints by Ultrasonic Signal Analysis   2004 October;22(5)
Evaluation of Flaws in Adhesively Bonded Joint using Ultrasonic Signal Analysis  2004 April;22(2)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.