Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-05.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 On the Fillet Weld-Induced Deformation Control by Applying the Tensioning Method

Journal of KWJS 2009;27(4):38-43.
Published online September 14, 2009.
장력법을 적용한 필릿용접변형 제어에 관한 연구
,
 
On the Fillet Weld-Induced Deformation Control by Applying the Tensioning Method
Joo-Sung Lee, Cheul-Ho Kim
Abstract
  As it has been well appreciated, the weld-induced deformation control is one of the most important issues from view point of efficiency in ship production. The weld-induced deformation is more serious in the case of thin plate block than in the case of relatively thick plate block, since, for example, heat affect zone of thin plates is wider than that of thick plates for the same heat input. Among weld-induced deformation, buckling deformation due to shrinkage and residual stress in weld line direction is one of the most serious deformation type. This paper is concerned with the controling the buckling deformation of thin plate fillet weld by applying the tensioning method. Weld experiments have been carried out for specimens with varying the magnitude and direction of tension load. The results are graphically represented to show the effect of tensioning method upon reducing the weld-induced deformation. From the present findings, its has been seen that tensioning method is one of the useful ways to control the weld-induced deformation of fillet weld of thin plates.
Key Words: Buckling deformation, Buckling mode, Residual stress, Tension load, Tensioning method, Thin plate, Fillet weld, Weld-induced deformation
TOOLS
METRICS Graph View
  • 1,461 View
  • 0 Download
Related articles


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI