Advanced Search  
JWJ > Volume 21(7); 2003 > Article
Journal of KWJS 2003 December;21(7) :42-48.
Published online December 25, 2003.
A Study on an Optimization of Welding Process Parameters by using an Analytic Solution for the Welding Angular Distortion
Se-Hean Lee
Correspondence:   Published online December 25, 2003
ABSTRACT
Welding distortion is a current issue in many industrial parts, especially for heavy industry such as shipbuilding, plant industry. The welding process has many processing parameters influencing welding angular distortion such as heat input power, welding speed, gas flow rate, plate thickness and the welded material properties, etc. In this work, the conventional local minimization concept was applied to find a set of optimum welding process parameters, consisted of welding speed, plate thickness and heat input, for a minimum angular distortion. An analytic solution for welding angular distortion, which is based on laminated plate theory, was also applied to investigate and optimize the welding process parameters. The optimized process parameters and the angular distortion for various parametric conditions could be easily found by using the local minimum concept.
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
953
View
0
Download
Related articles
Optimization of Weld-bonding Process Conditions of Dissimilar Materials using Delta Spot Welding  2019 June;37(3)
A Study on optimization of welding process parameters for J-Groove dissimilar metal weld repair of pressurizer heater sleeve in nuclear power plants  2015 February;33(1)
Recent Study in Variation of Welding Materials for Overlay Welding  2013 December;31(6)
Optimization of Robot Welding Process of Subassembly Using Genetic Algorithm in the Shipbuilding  2009 April;27(2)
A Study on the Optimization of IR Laser Flip-chip Bonding Process Using Taguchi Methods  2008 June;26(3)
Optimization of Weld-bonding Process Conditions of Dissimilar Materials using Delta Spot Welding  2019 June;37(3)
A Study on optimization of welding process parameters for J-Groove dissimilar metal weld repair of pressurizer heater sleeve in nuclear power plants  2015 February;33(1)
Recent Study in Variation of Welding Materials for Overlay Welding  2013 December;31(6)
Optimization of Robot Welding Process of Subassembly Using Genetic Algorithm in the Shipbuilding  2009 April;27(2)
A Study on the Optimization of IR Laser Flip-chip Bonding Process Using Taguchi Methods  2008 June;26(3)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.