Estimation of Fatigue Strength in Resistance Spot Weldment of the Vehicle Body
손광재, 양영수, 조성규, 장상균



Correspondence:   Published online April 25, 2002
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
947
View
0
Download
Related articles
Effects of Electrode Face Thickness on Resistance Spot Weldability of Aluminium Alloy 6061  2020 February;38(1)
Effects of Electrode Face Radius and Force on Resistance Spot Weldability of Aluminium Alloy 6061  2018 December;36(6)
Evaluation of Failure Mode and Strength on Baking Time of Adhesive for Hybrid Joining  2011 December;29(6)
Optimization of Fuzzy Controller for Constant Current of Inverter DC Resistance Spot Welding Using Genetic Algorithm  2010 October;28(5)
Estimation of Fatigue Life in Butt-Welded Zone of SM45C Steel Rod  2008 June;26(3)
Effects of Electrode Face Thickness on Resistance Spot Weldability of Aluminium Alloy 6061  2020 February;38(1)
Effects of Electrode Face Radius and Force on Resistance Spot Weldability of Aluminium Alloy 6061  2018 December;36(6)
Evaluation of Failure Mode and Strength on Baking Time of Adhesive for Hybrid Joining  2011 December;29(6)
Optimization of Fuzzy Controller for Constant Current of Inverter DC Resistance Spot Welding Using Genetic Algorithm  2010 October;28(5)
Estimation of Fatigue Life in Butt-Welded Zone of SM45C Steel Rod  2008 June;26(3)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.