A Study on Rotating Arc Using Hollow Shaft Motor
김철희, 나석주

Correspondence:   Published online October 25, 2000
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
780
View
0
Download
Related articles
A Study on Prediction of Fatigue Life using MFC Sensors  2013 December;31(6)
A Study on 3-D Information Extraction using Single X-ray Image  2011 February;29(1)
A Study on the Buckling in Fillet Welds of Sheets  2009 June;27(3)
A Study on Monitoring for Process Parameters Using Isotherm Radii  2006 October;24(5)
A Study on the Erosion-Resistant Cermet Film Coating Using the Detonation Spray Method   2001 February;19(1)
A Study on Prediction of Fatigue Life using MFC Sensors  2013 December;31(6)
A Study on 3-D Information Extraction using Single X-ray Image  2011 February;29(1)
A Study on the Buckling in Fillet Welds of Sheets  2009 June;27(3)
A Study on Monitoring for Process Parameters Using Isotherm Radii  2006 October;24(5)
A Study on the Erosion-Resistant Cermet Film Coating Using the Detonation Spray Method   2001 February;19(1)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.