Mechanism of Hot Cracking in High Strength Al Welds
이창희, 조성석

Correspondence:   Published online June 25, 1996
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
689
View
0
Download
Related articles
Nucleation Behavior of Acicular Ferrite in 1 GPa Class High Strength Steel Weld Metal  2019 February;37(1)
Characteristics of Sulfide Stress Cracking of High Strength Pipeline Steel Weld by Heat Input  2018 June;36(3)
Recent Studies of the Laser Cladding of High Entropy Alloys   2017 August;35(4)
The Effects of Microstructure on Cold Crack in High-Strength Weld Metals  2014 February;32(1)
Evaluation of Hydrogen Delayed Fracture for High Strength Steels and Weldments  2011 December;29(6)
Nucleation Behavior of Acicular Ferrite in 1 GPa Class High Strength Steel Weld Metal  2019 February;37(1)
Characteristics of Sulfide Stress Cracking of High Strength Pipeline Steel Weld by Heat Input  2018 June;36(3)
Recent Studies of the Laser Cladding of High Entropy Alloys   2017 August;35(4)
The Effects of Microstructure on Cold Crack in High-Strength Weld Metals  2014 February;32(1)
Evaluation of Hydrogen Delayed Fracture for High Strength Steels and Weldments  2011 December;29(6)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.