Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 A Study on the Stress Corrosion Cracking Behaviors for Weld Joint of Steel with Various pH Values in Synthetic Sea Water

Journal of KWJS 1995;13(1):78-88.
Published online March 27, 1995.
인공해수의 pH에 따른 강 용접부의 응력 부식균열거동에 관한 연구
, ,
 
A Study on the Stress Corrosion Cracking Behaviors for Weld Joint of Steel with Various pH Values in Synthetic Sea Water
유효선, 나의균, 정세희