Effect of Weld Residual Stress on Fatigue Analysis of Nozzle
Sang-Chul Kim*, Man-Won Kim**
*Dept. of Occupational Health & Safety Engineering, Semyung University, Jecheon 390-711, Korea
**Central Research Institute, KHNP, Daejeon 305-343, Korea
Correspondence: Sang-Chul Kim  Email: sckim@semyung.ac.kr
  Published online February 27, 2014
ABSTRACT
Although the fatigue design curve of ASME Code has enough margin with respect to alternating stress and cycles, the welding residual stress(WRS) should be included in fatigue analysis. In this paper, WRS distribution in a nozzle with dissimilar metal weldment was obtained by finite element analysis and was added in fatigue analysis. The fatigue analysis was performed by following the ASME Code including thermal and stress analysis applying with postulated 30 transient conditions. The calculated results of a cumulative fatigue usage factors(CUF) were compared for the case of the models with or without WRS effects. The results showed that the CUF at weldment and heat affected zone was affected by the WRS.
Keywords: Fatigue analysis | Cumulative usage factor | Dissimilar metal weld | Finite element method | weld residual stress
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1
Crossref
1,077
View
7
Download
Related articles
Effect of Weld Elastic Modulus on Simulation of Stress Concentration and Fatigue Life for Boiler Vessel  2016 October;34(5)
Effect of the welding residual stress redistribution on impact absorption energy  2015 February;33(1)
The Study of Measurement of Residual Stress for Pipe Weldments of Power Plant  2012 April;30(2)
A Study on the Weld-induced Residual Stress Analysis at FPSO Moon Pool Structure  2011 June;29(3)
Effect of Residual Stresses Depends on Transverse Cracks in Thick Steel Weldments  2008 August;26(4)
Effect of Weld Elastic Modulus on Simulation of Stress Concentration and Fatigue Life for Boiler Vessel  2016 October;34(5)
Effect of the welding residual stress redistribution on impact absorption energy  2015 February;33(1)
The Study of Measurement of Residual Stress for Pipe Weldments of Power Plant  2012 April;30(2)
A Study on the Weld-induced Residual Stress Analysis at FPSO Moon Pool Structure  2011 June;29(3)
Effect of Residual Stresses Depends on Transverse Cracks in Thick Steel Weldments  2008 August;26(4)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.