ABSTRACT
Magnesium alloy is used on parts of aircraft and electronic equipment because of the highest specific strength among the common metal materials. Recently, studies about appling magnesium alloy sheet to automotive bodies are on the increase rapidly. For application to automotive bodies, researches about characteristics of resistance spot welding of magnesium alloy sheet are essential. Magnesium alloy has low boiling point, so getting sound bead shape is difficult when appling varies welding processes. Resistance spot welding is also particular about setting optimum welding conditions because of spatter generation, pores and cracks occurrence in nugget. And life of electrodes is very short because of alloying with copper that main material of electrodes. This requires frequent dressing and replacement of electrodes and decrease in productivity of resistance spot welding on magnesium alloy. Therefore in this study, for effective analysis of changes in tensile shear load and nugget size during electrode life test, evaluate detail characteristics of resistance spot welding on magnesium alloy sheet using dome type electro
Keywords: Resistance spot welding | AZ31 | Mg alloy | Dome type electrode
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
2
Crossref
1,318
View
11
Download
Related articles
Effects of Electrode Face Thickness on Resistance Spot Weldability of Aluminium Alloy 6061  2020 February;38(1)
Resistance Spot Welding Characteristics of Mg Alloy Applying Current Waveform Control  2014 April;32(2)
Resistance Spot Welding Characteristics of Mg Alloy Using Process Tape  2013 June;31(3)
Monitoring of Resistance Spot Welding Processes  2012 February;30(1)
Dynamic Model for Electrode Expansion in Resistance Spot Welding Machines  2011 April;29(2)
Effects of Electrode Face Thickness on Resistance Spot Weldability of Aluminium Alloy 6061  2020 February;38(1)
Resistance Spot Welding Characteristics of Mg Alloy Applying Current Waveform Control  2014 April;32(2)
Resistance Spot Welding Characteristics of Mg Alloy Using Process Tape  2013 June;31(3)
Monitoring of Resistance Spot Welding Processes  2012 February;30(1)
Dynamic Model for Electrode Expansion in Resistance Spot Welding Machines  2011 April;29(2)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.