ABSTRACT
The latest research & development trend on friction stir welding and friction stir processing technologies presented in the international symposium, ‘Friction Stir Welding & Processing Ⅶ’. Papers and presentations about high temperature materials such as advanced high strength steel, stainless steel and titanum alloy shoot up this year. Papers on modeling of metal flow and control of process parameters also increased. The FSP technologies for manufacturing of carbon materials reinforced metal matrix composites were reported, too.
Keywords: Friction stir welding | Friction stir processing | Modeling | High temperature materials | Light metals
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
1,156
View
8
Download
Related articles
Trends of Technology Development of Friction Stir Welding Machine  2016 June;34(3)
Recent R&D status on friction stir welding of Ti and its alloys  2015 April;33(2)
Influence of Surface Roughness of Tools on the Friction Stir Welding Process  2014 December;32(6)
Friction Stir Welding of Ferritice Stainless Steel  2014 April;32(2)
Recent Trends of Friction Stir Welding of Titanium  2013 April;31(2)
Trends of Technology Development of Friction Stir Welding Machine  2016 June;34(3)
Recent R&D status on friction stir welding of Ti and its alloys  2015 April;33(2)
Influence of Surface Roughness of Tools on the Friction Stir Welding Process  2014 December;32(6)
Friction Stir Welding of Ferritice Stainless Steel  2014 April;32(2)
Recent Trends of Friction Stir Welding of Titanium  2013 April;31(2)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.