Technology on Arc Welding Machine of Aluminum by Digital Control
Chang-Je LEE, Yu-Chan KIM, Jong-Do KIM
R&D Institute, BEST F.A, Changwon 641-290, Ko
Division of Marine Engineering, Korea Maritime University, Busan 606-791, Korea
Correspondence: Chang-Je LEE  Email: lab@bestfa.co.kr
  Published online June 4, 2013
ABSTRACT
Recently, welding technology of nonferrous metals which were difficult to implement by arc welder has become available through digitalization of arc welding machine. Among them, the welding quality improvement of aluminum welding is very noticeable. These results increase the arc stability by controlling arc current and voltage waveform precisely, and control wire feed speed by synchronizing with arc current which the feed rate of filler wire is controlled by a precise motor control of servomotor and not by a simple constant speed feeding. Not only through the hardware digitalization of arc welding machine but also through advance of software of arc welding, it became possible to implement a certain level of welding quality by a simple operation. These led to CMT welding process implementation which requires low heat input than current arc welding and highly increased the applicability of the aluminum welding.
Keywords: Aluminum | Digital | Arc stability | Inverter | Synergic line | CMT
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1
Crossref
1,031
View
0
Download
Related articles
High Current Arc Welding Technology of Aluminum Alloy  2013 February;31(1)
Spot Welding of Aluminum Alloys Using Servogun  2004 August;22(4)
Laser-Arc Hybrid Welding Process of Aluminum Alloy  2004 April;22(2)
Autogenous Welding Properties of Aluminum Alloys by Multi Wavelength Laser  2004 February;22(1)
Laser Welding of Aluminum Alloys   2000 April;18(2)
High Current Arc Welding Technology of Aluminum Alloy  2013 February;31(1)
Spot Welding of Aluminum Alloys Using Servogun  2004 August;22(4)
Laser-Arc Hybrid Welding Process of Aluminum Alloy  2004 April;22(2)
Autogenous Welding Properties of Aluminum Alloys by Multi Wavelength Laser  2004 February;22(1)
Laser Welding of Aluminum Alloys   2000 April;18(2)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.