Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-05.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Active Metal Brazing Applied to Joining of ZrO2-Ti Alloy

J Weld Join > Volume 30(3); 2012 > Article
Journal of KWJS 2012;30(3):38-43.
DOI: https://doi.org/10.5781/KWJS.2012.30.3.38    Published online July 18, 2012.
ZrO₂-Ti합금의 활성금속 브레이징
, , ,
 
Active Metal Brazing Applied to Joining of ZrO2-Ti Alloy
Se-Ho Kee, Sang-Yoon Park, Jae-Pil Jung, Won-Joong Kim
Abstract
  In this study, active metal brazing methods for ZrO₂ and Ti alloy were discussed. To get a successful metal-ceramic bonding, various factors (melting temperature, corrosion, sag resistance, thermal expansion coefficient etc. of base materilas and filler metal) should be considered. Moreover, in order to clarify bonding between the metal and ceramic, the mechanism of the interfacial structure of the joints should be identified. The driving force for the formation of metal and ceramic interfaces is the reduction of the free energy which occurs when their contact becomes complete. Interfacial bonding depends on the material combinations and the bonding processes. This study describes the bonding between ceramic and metal in an active metal brazing.
Key Words: Vibration, Fatigue, Fracture, Intermetallic compound, Pb-free solder
TOOLS
METRICS Graph View
  • 0 Crossref
  •    
  • 1,844 View
  • 0 Download
Related articles

Gas Metal Arc Welding of Aluminum Alloys 1994 March;12(1)



ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI