Analysis of Pulsed GMAW Using Force-Displacement Model
Arif Nabeel, LeeJae Hak, YooChoong Don


Correspondence:   Published online March 12, 2009
ABSTRACT
  In order to determine the One-Drop One-Pulse (ODOP) condition of the pulsed gas metal arc (GMA) welding, the drop detaching phenomenon during the peak time is investigated using the force-displacement model. The drop detaching criterion is established based on the displacement of the pendant drop, and the forces exerted on the drop are calculated using the Modified Force Balance Model (MFBM). The effects of wire melting on the drop size and force are included in the force-displacement model. While the peak current has most significant effects on the drop detaching time, the initial drop mass prior to the peak time also influences drop transfer. The calculated results show good agreements with the experimental data, which implies that the ODOP condition can be predicted using the force-displacement method.
Keywords: Pulsed GMAW;Force-displacement model;ODOP;MFBM;Wire melting
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,020
View
0
Download
Related articles
Analysis of Weldment by Using Finite Element Method(1) - Heat Flow in Weldment -  2011 April;29(2)
Analysis of Metal Transfer Using Dynamic Force Balance Model in GMAW   2001 August;19(4)
Analysis of Fatigue Strength in Expansion Joint Weldment of Bridge   1998 August;16(4)
Analysis of Restraint Stress Acting on the Weldment   1997 February;15(1)
Analysis of Weldment by Using Finite Element Method(1) - Heat Flow in Weldment -  2011 April;29(2)
Analysis of Metal Transfer Using Dynamic Force Balance Model in GMAW   2001 August;19(4)
Analysis of Fatigue Strength in Expansion Joint Weldment of Bridge   1998 August;16(4)
Analysis of Restraint Stress Acting on the Weldment   1997 February;15(1)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.