1 Trends of Technology Development of Friction Stir Welding Machine   
Young-Pyo Kim, Cheol-Hee Kim, Young-Gon Kim, Sung-Min Joo
Journal of Welding and Joining:1-5.  Publication Date (Web): June 30, 2016   Cited by 1
                  PDF Links
 
6 Effect of Circumferential Tool Path Control on Friction Stir Spot Welding of Al/Fe Dissimilar Metal Joint   
Jin Young Yoon, Cheolhee Kim, Sehun Rhee
Journal of Welding and Joining:6-11.  Publication Date (Web): June 30, 2016
                  PDF Links
 
12 A study on an Interface Tracking Algorithm in Friction Stir Welding based on Computational Fluid Dynamics Analysis   
Su-Deok Kim, Suck-Joo Na
Journal of Welding and Joining:12-16.  Publication Date (Web): June 30, 2016   Cited by 1
                  PDF Links
 
17 Effect of Tool Plunge Depth on Weldability of Dissimilar Al5083-O/DP590 Friction Spot Joint   
Su-Ok Jeong, Han-Sur Bang, Hee-Seon Bang
Journal of Welding and Joining:17-22.  Publication Date (Web): June 30, 2016   Cited by 1
                  PDF Links
 
23 Optimizing the Friction Stir Spot Welding Parameters to Attain Maximum Strength in Al/Mg Dissimilar Joints   
Manickam Sundaram, Balasubramanian Visvalingam
Journal of Welding and Joining:23-30.  Publication Date (Web): June 30, 2016   Cited by 1
                  PDF Links
 
31 Latest Joining Technology of Metal and Plastic   
Youngsik Kim, Sangcheol Kil
Journal of Welding and Joining:31-39.  Publication Date (Web): June 30, 2016   Cited by 2
                  PDF Links
 
40 Short Circuit Waveform Control Type SMAW Welding Power Source Development and Characteristic Evaluation   
Hyun-Min Yang, Hoi-Soo Ryoo, Soong-Keun Hyun
Journal of Welding and Joining:40-46.  Publication Date (Web): June 30, 2016   Cited by 1
                  PDF Links
 
47 Low Cycle Fatigue Performance of 304L Stainless Steel Weldments   
JaeHyoen Hwang, DongJin Oh, DoYoung Lee, MinSung Chun, Myung-Hyun Kim
Journal of Welding and Joining:47-51.  Publication Date (Web): June 30, 2016
                  PDF Links
 
52 Effects of Post Weld Heat Treatment on Microstructures of Alloy 617 and 263 Welds for Turbines of HSC Power Plants   
Jeong Kil Kim, Deog Nam Shim, Hae Ji Park
Journal of Welding and Joining:52-60.  Publication Date (Web): June 30, 2016
                  PDF Links
 
61 A Study of Characteristics on the Dissimilar Metals (Alloy Steel : A387 Gr. 91 - Carbon Steel : A516 Gr. 70) Welds Made with FCA Multiple Layer Welding : Part 1   
Tae Woo Shin, Bok Su Jang, Jin Hyun Koh
Journal of Welding and Joining:61-68.  Publication Date (Web): June 30, 2016
                  PDF Links
 
69 A Study of Characteristics on the Dissimilar Metals (ASTM Type 316L - Carbon Steel : ASTM A516-70) Welds Made with FCA Multiple Layer Welding   
Se Cheol Kim, Jun Hyeok Hyun, Tae Woo Shin, Jin Hyun Koh
Journal of Welding and Joining:69-76.  Publication Date (Web): June 30, 2016
                  PDF Links
 
e-submission
endonote style file
JWJ
vol: Issue: Page:
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.