28 A Study for Brittle Crack Prevention and Fatigue Life Improvement using a Welded Stiffener   
Tae-Woo Kang, Myung-Hyun Kim
Journal of Welding and Joining:28-33.  Publication Date (Web): December 26, 2018
                  PDF Links
 
41 A Study of Fatigue Crack Growth Behaviour for Ferrite-Bainite Dual Phase Steel   
Deok-Geun Kim, Dong-Pil Cho, Dong-Jin Oh, Myung-Hyun Kim
Journal of Welding and Joining:41-46.  Publication Date (Web): February 29, 2016
                  PDF Links
 
45 Fatigue Crack Growth Characteristics of 9% Ni Steel Welded Joint for LNG Storage Tank at Low Temperature
Jae-Hoon Kim, Kyue-Taek Shim, Young-Kyun Kim, Byoung-Wook Ahn
Journal of Welding and Joining:45-50.  Publication Date (Web): November 5, 2010
PDF Links
 
1 |
e-submission
endonote style file
JWJ
vol: Issue: Page:
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.