Journal of KWJS. 1998;16(4):63-72. Published online August 25, 1998.
- The Effect of Current Pulsing Parameters on the Spatter Generation Rate during CO₂ Shielded Gas Metal Arc Welding
-
강덕일, 최재호, 장영섭, 김용석
-