A Study on the Microstructure and Mechanical Properties of the Coarse Grain Heat Affected Zone in EH40 Grade High Strength Structural Steels
Seonghoon Jeong, Seunglae Hong, JunSeok Seo, Ji-Hee Son, Hyung Goun Joo
J Weld Join. 2022;40(5):410-415.