Previous issues
Volume 33 Issue 2
-
Special Issues
Recent R&D status on friction stir welding of Ti and its alloys
- Duck-soo Kang, Kwang-jin Lee
- J Weld Join. 2015;33(2):1-7.
-
Special Issues
Evaluation of mechanical properties on friction stir lap jointed Al6061/HT590 alloys
- Eun-Hye Kim, Kwang-Jin Lee, Kuk-Hyun Song
- J Weld Join. 2015;33(2):8-13.
-
Special Issues
Theoretical background discussion on variable polarity arc welding of aluminum
- Jungho Cho, Jungjae Lee, Seunghwan Bae, Yongki Lee, Kyungbae Park, Yongjun Kim, Junkyung Lee
- J Weld Join. 2015;33(2):14-17.
-
Special Issues
Evaluation and solution of noise making weldment in automotive body
- Jungho Cho, Jungjae Lee, Seunghwan Bae, Yongki Lee, Kyungbae Park, Yongjun Kim, Semin Moon
- J Weld Join. 2015;33(2):18-22.
-
Research Papers
Optimization of arc brazing process parameters for exhaust system parts using box-behnken design of experiment
- Yong Kim, Pyeong-Won Park, Ki-Young Park, Jin-Chul Ryu
- J Weld Join. 2015;33(2):23-31.
-
Research Papers
Numerical analysis on the welding residual stress and fracture toughness of the heavy thick steel welded joints by welding processes
- HanSur Bang, HeeSeon Bang
- J Weld Join. 2015;33(2):32-39.
-
Research Papers
The effect of ultrasonic nano crystal surface modification for mitigation of the residual stress after weld inlay on the alloy 82/182 dissimilar metal welds of reactor vessel in/outlet nozzles
- Hong Seok Cho, Ik Keun Park, Kwang Woon Jung
- J Weld Join. 2015;33(2):40-46.
-
Research Papers
A comparative study of constant current control and adaptive control on electrode life time for resistance spot welding of galvanized steels
- Jeong-Chul Seo, Il-Dong Choi, Hong-Rea Son, Changwook Ji, Chiho Kim, Sung-Bu Suh, Jinseok Seo, Yeong-Do Park
- J Weld Join. 2015;33(2):47-55.
-
Research Papers
Characterization of resistance spot welded Al5052/DP590 dissimilar materials and
processing optimization
- Beom-Ji Jo, Ji-Sun Kim, Hyo-Sang Yoo, In-Ju Kim, Seong-Hui Lee, Young-Gon Kim
- J Weld Join. 2015;33(2):56-61.
-
Research Papers
A study on reduction of pre-crack deviation in CTOD specimen using reverse bending method
- Sehwan Jeong, Dong-Hwan Park, Hyeon-su Kim, Sang-beom Shin, Tae-jong Park
- J Weld Join. 2015;33(2):62-68.
-
Research Papers
A study on tensile shear characteristics for weld-bonded 1.2GPa grade TRIP steels with changes in nugget diameter for automotive body application
- Ildong Choi, Jiyoun Park, Jae-Won Kim, Mun-jin Kang, Dong-Cheol Kim, Jun-Ki Kim, Yeong-Do Park
- J Weld Join. 2015;33(2):69-77.
-
Research Papers
Finite element analysis for joining glass fiber reinforced plastic and aluminium alloy sheets
- Hae-Yong Cho, Dongbum Kim
- J Weld Join. 2015;33(2):78-84.
-
Research Papers
The characteristics of bead welding on steel with process parameter during the laser-arc hybrid welding(Ⅰ) - Effect of flow rate of shield gas and distance between laser and arc -
- Jong-Do Kim, Gi-Hoon Myung, Moo-Keun Song, Jae-Hwan Oh, Jeong Suh
- J Weld Join. 2015;33(2):85-90.
-
Research Papers
The characteristics of bead welding on steel with process parameter during the laser-arc hybrid welding(Ⅱ) - Effect of heat input parameters -
- Jond-Do Kim, Gi-Hoon Myung, In-Duck Park
- J Weld Join. 2015;33(2):91-96.