Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-05.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 100 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 101 Analysis of Welding Phenomena and Effect of Short Circuit Current Rise Slope in the High Speed CO₂Welding of Steel Sheets

Journal of KWJS 2005;23(5):14-19.
Published online November 11, 2005.
[기술논문] CO₂ 박판 고속용접에서 용접현상 분석과 전류상승기울기의 영향
, ,
 
Analysis of Welding Phenomena and Effect of Short Circuit Current Rise Slope in the High Speed CO₂Welding of Steel Sheets
Young-Sam Kim, Hoi-Soo Ryoo, Hee-Jin Kim
Abstract
In high speed CO₂ welding, it has been known to produce no sound bead with undercut or humping bead. In this study welding phenomena through synchronized high speed camera and output welding voltage and current waveform has been analyzed. For the purpose to improve a welding bead, effect of short circuit current rise slope has been examined. With commercial power source it was produced no sound bead by instantaneous short circuit, long arc period and stubbing at welding speed 2.5㎜/min. Humping bead or undercut were showed by instantaneous short circuit and long arc period. Also, the weld bead was not formed during the long short circuit period after stubbing start and long arc extinguishment period after wire sticking by failure of arc regeneration, because the droplet was not transferred to weld pool. With increasing short circuit current rise slope the frequency of stubbing was decreased and the normal short circuit rate was increased. A control of short circuit current rise slope was effective factor in high speed welding.
TOOLS
METRICS Graph View
  • 1,578 View
  • 0 Download
Related articles

Characteristic of Welding Rotational Deformation in Laser Welding of Thin Steel Sheet2018 December;36(6)



ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI