Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2025-02.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 100 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 101 Nondestructive Evaluation of Ceramic/Metal Interface Using the V(z) Curve of Scanning Acoustic Microscope

Journal of KWJS 2005;23(2):59-65.
Published online May 12, 2005.
[연구논문]초음파현미경에서 V(z)곡선을 이용한 세라믹/금속 접합계면의 비파괴평가
, , ,
 
Nondestructive Evaluation of Ceramic/Metal Interface Using the V(z) Curve of Scanning Acoustic Microscope
Ik-Keun Park, Chul-Ku Lee, Dong-Su Cho, Yong-Kwon Kim
Abstract
A leaky surface acoustic wave (LSAW) velocity was measured using a scanning acoustic microscope on the ceramic/metal interface in order to investigate material properties. The inverse Fourier transform (IFFT) of the V(z) curve contains the reflectance function of a liquid-specimen interface. So, the longitudinal, transverse, and Rayleigh wave velocities for each layer are obtained by the inversion of the V(z) curve at the same time. This paper contains mainly the experimental procedure for measurements of the LSAW velocity, and the results obtained for the velocity variation of individual layer after the thermal shock. It is shown that this method is useful in measuring the material properties under external stress.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2025 by The Korean Welding and Joining Society.

Developed in M2PI