Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Prparation, Structure and Tribological Properties of Al-based Quasicrystalline Coatings Deposited by Thermal Spray Techniques

Journal of KWJS 2003;21(2):9-19.
Published online April 25, 2003.
용사피복법에 의한 준결정코팅층의 제조 및 특성 평가
, , , , , ,
 
Prparation, Structure and Tribological Properties of Al-based Quasicrystalline Coatings Deposited by Thermal Spray Techniques
김유찬, 김도형, 김도향, 김원태, 안효석, 이상목, E Fleury