Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2025-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 100 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 101 A Study on Pulsed Nd:YAG Laser Welding of Electron Gun in Braun Tubes(1)-Characteristics of Beam Output Energy and Optical Parameters-

Journal of KWJS 2002;20(4):119-127.
Published online August 26, 2002.
브라운관 전자총 부품의 펄스 Nd:YAG 레이저 용접에 관한 연구(1)-빔의 출력특성과 광학변수-
, ,
 
A Study on Pulsed Nd:YAG Laser Welding of Electron Gun in Braun Tubes(1)-Characteristics of Beam Output Energy and Optical Parameters-
김종도, 하승협, 조상명