A Study on the GMA Welding Characteristics of Al5083-O Aluminum Alloy According to the Shield Gas Mixing Ratio and Heat Input
정재강, 양훈승, 이동길


Correspondence:   Published online April 25, 2002
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
831
View
0
Download
Related articles
A Review on the Characteristics of Laser Welding with Filler Wire According to Process Parameters Controlling the Heat Input and Wire Feeding  2021 April;39(2)
Evaluation of Gas Metal Arc Welding Characteristics according to Contact Tip Materials  2014 December;32(6)
A Study on the Welding Distortion Analysis According to Rib Height in Fillet Welding  2013 December;31(6)
A Study on the Welding Characteristics of Hastelloy C-276 using a Continuous Wave Nd:YAG Laser  2008 October;26(5)
A Study on the Adhesive Characteristics of Nano Scale Particles Considering Asperity Interaction  2008 February;26(1)
A Review on the Characteristics of Laser Welding with Filler Wire According to Process Parameters Controlling the Heat Input and Wire Feeding  2021 April;39(2)
Evaluation of Gas Metal Arc Welding Characteristics according to Contact Tip Materials  2014 December;32(6)
A Study on the Welding Distortion Analysis According to Rib Height in Fillet Welding  2013 December;31(6)
A Study on the Welding Characteristics of Hastelloy C-276 using a Continuous Wave Nd:YAG Laser  2008 October;26(5)
A Study on the Adhesive Characteristics of Nano Scale Particles Considering Asperity Interaction  2008 February;26(1)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.           Developed in M2PI