Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Characteristics of Liquid Phase Diffusion Bonded Joints Using Newly Developem Ni-3Cr-4Si-3B Insert Metal of Heat Resistant Alloy

Journal of KWJS 2000;18(6):62-67.
Published online December 25, 2000.
신개발 Ni-3Cr-4Si-3B 삽입금속으로 액상확산접합한 내열주강 접합부의 특성
 
Characteristics of Liquid Phase Diffusion Bonded Joints Using Newly Developem Ni-3Cr-4Si-3B Insert Metal of Heat Resistant Alloy