Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-07.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 100 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 101 A Study of Weld Fusion Zone Phenomena in Austenitic Stainless Steels(2) - Effect of Nitrogen on Microstructural Evolution and Hot Cracking Susceptibility of GTA Welds in STS 304 -

Journal of KWJS 2000;18(1):59-69.
Published online February 25, 2000.
오스테나이트계 스테인리스강 용접부의 금속학적 현상에 관한 연구(2) - STS 304 용접부 조직특성 및 고온균열 감수성에 미치는 질소의 영향 -
,
 
A Study of Weld Fusion Zone Phenomena in Austenitic Stainless Steels(2) - Effect of Nitrogen on Microstructural Evolution and Hot Cracking Susceptibility of GTA Welds in STS 304 -
이종섭, 김숙환


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI