Effect of Heterogeneous Microstructure on the Fracture Toughness of Weld Metal
정현호, 김철만, 김형식, 김우식, 홍성호




Correspondence:   Published online April 26, 1999
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,035
View
0
Download
Related articles
Correlation Between HAZ Microstructure and Low Temperature Impact Toughness of Bainitic Steel Plates  2021 June;39(3)
Effect of Microstructure on Low-Temperature Impact Toughness of Multi-Pass Weld Metal of 1 GPa Class High Strength Steel  2021 June;39(3)
Effect of Aluminum, Nitrogen and Silicon Content on the Toughness of C-Mn Steel Weld Heat Affected Zone  2020 February;38(1)
Effect of Tensile Properties and Microstructure on the Heat Input of Ni-Doped High Manganese Welding Wire  2018 February;36(1)
The Effects of PWHT on Tensile Properties and Microstructures for Laser Welds of Ti-6Al-4V Alloys   2017 August;35(4)
Correlation Between HAZ Microstructure and Low Temperature Impact Toughness of Bainitic Steel Plates  2021 June;39(3)
Effect of Microstructure on Low-Temperature Impact Toughness of Multi-Pass Weld Metal of 1 GPa Class High Strength Steel  2021 June;39(3)
Effect of Aluminum, Nitrogen and Silicon Content on the Toughness of C-Mn Steel Weld Heat Affected Zone  2020 February;38(1)
Effect of Tensile Properties and Microstructure on the Heat Input of Ni-Doped High Manganese Welding Wire  2018 February;36(1)
The Effects of PWHT on Tensile Properties and Microstructures for Laser Welds of Ti-6Al-4V Alloys   2017 August;35(4)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society.           Developed in M2PI