Journal of KWJS 1999;17(1):45-51. Published online February 25, 1999. |
|
Corrosion Assessment of Al/Fe Dissimilar Metal Joint2014 August;32(4)
Vacuum Plasma Sprayed NiTiZrSiSn Coating2007 August;25(4)
Optimization of the Plasma Spray Coating Parameters of Ni-5%AI Alloy Powder 2002 October;20(5)
The Microstructure of Fiber Reinforced Plasma Sprayed Coatings2002 August;20(4)
Properties of Plasma Sprayed Al₂O₃/SS316 Graded Coatings 2002 April;20(2)