Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 A Study on the effect of the multi-pass SMAW welding on the characteristic of the underwater welding areas

Journal of KWJS 1998;16(4):55-62.
Published online August 25, 1998.
SMAW 수중 다층용접시 용접부 특성에 관한 연구
, , , , ,
 
A Study on the effect of the multi-pass SMAW welding on the characteristic of the underwater welding areas
최기용, 이상율, 이보영, 이병훈, 이상용, 박성두