Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 The Studies on the Prediction of Residual Stresses by Thermal Elasto-Plastic Analysis and its Effect for Circumferential Welded Cylinder

Journal of KWJS 1997;15(5):115-123.
Published online October 27, 1997.
열탄소성 해석에 의한 원주용접 원통관의 잔류응력 예측과 그 영향에 대한 연구
,
 
The Studies on the Prediction of Residual Stresses by Thermal Elasto-Plastic Analysis and its Effect for Circumferential Welded Cylinder