Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-06.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 100 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 101 A Study on Transverse Cracking and Fatigue Properties of 50mm Thick FCAW Weld Metal ; Effects of Preheating and Interpass Temperature

Journal of KWJS 1997;15(3):56-64.
Published online June 25, 1997.
FCAW 50t 후판용접에 있어 예열 및 층간온도 변화에 따른 횡크랙 발생과 피로특성에 관한 연구
,
 
A Study on Transverse Cracking and Fatigue Properties of 50mm Thick FCAW Weld Metal ; Effects of Preheating and Interpass Temperature
이해우, 강성원
TOOLS
METRICS Graph View
  • 1,238 View
  • 1 Download
Related articles

A Study on Wear Properties of Plasma sprayed Cr3C2-NiCr Coating at High Tempeature 1993 December;11(4)



ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI